1. Products Description

 OP modified ethylene propylene diene monomer (EPDM) resins are ethylene-propylene copolymer rubber and thermoplastic PU vulcanized by heating to made of resin particles

2. Products Form

 Color: black              Shape: Semi-granular

3.Physical Properties

OP-105 has good tensile strength (≥ 12Mpa), rebound performance and excellent crack resistance in low-temperature( -40 °C) still maintain good flexibility.OP-105 has a good mobile performance,easy to extrusion processing. 

Q/SZE105-2009

 Item

OP-105

 EPDM content/%

30

   Density(g/cm3)

1.05

Tension strength/Mpa

≥12

    Elongation/%

≥450

  Embrittlement temperature °C

-40

     Melting Point/°C

105

 4.Recommendations for extrusion conditions (For reference only)

 

Item

Temperature Range

Item

Temperature Range

Barrel rear

70-80°C

Die between

100-105°C

Barrel Central

100-105°C

Die left

120-130°C

Barrel Anterior

110-120°C

Die right

120-130°C

5.Application Range

OP-105 is raw materials of roofing waterproof membrane.

 

 

Modified EPDM resin(OP-105)

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.