1.round bar diameter:8-2000mm. 2.plate/sheet thickness:2-200mm. 3.forgings weight:0.5-10000Kg. 4.pipe/tube OD80-3500mm.
1.Type analysis
C | Si | Mn | Cr | Mo | W | C0 | Cu | Fe | Nb/Ta | Ni |
0.03 | 1.0 | 2 | 29.5 | 5 | 2.5 | 5 | 1.7 | 15 | 0.7 | balance |
2.Description
HASTELLOY G-30 alloy is a high chromium nickel-base alloy which shows superior corrosion resistance over most other nickel- and iron-base alloys in commercial phosphoric acids as well as many complex environments containing highly oxidizing acids such as nitric/hydrochloric, nitric/hydrofluoric and sulfuric acids. The resistance of G-30 alloy to the formation of grain boundary precipitates in the heataffected zone makes it suitable for use in the as-welded condition.
Hastelloy G-30/N06030/Alloy G30 corrosion-resisting superalloy wires