1.material: ZrO2 2.method of moulding: Thermal casting/dry press/ extrusion 3.clour:white /light yellow 4.high quality
1.material: ZrO2
2.ethod of moulding: Thermal casting/dry press/extrusion
3.colour:white /light yellow
4.Sintering temperature:1580oC
5.Material characteristics: Density 6.05g/ cm3, Elasticity 205GPa HRA&ge80
6.Surface finish: Ra0.3 &simRa0.8&mum
7.Packing: pack with carton and ship with wooden case
8.Produce products according to molds or drawings provided by the client and quote according the data of the products.
Item | Test Condition | Unit&Symbol | Zirconia Ceramic |
The main chemical ingredient | ZrO2: 95% Y2O3: 5% | ||
Bulk Density | g/cm3 | 6 | |
Maximum Use Temperature | 1300°C | ||
Water absorption | % | 0 | |
ROHS Hardness | HRA | ≥83 | |
Compressive Strength | 20° C | Kgf/cm2 | 25000 |
Fracture Toughness | Map.m3/2 | 6 - 8 | |
Coefficient of thermal expansion | /°C | 9.5*10-6 | |
Thermal Shock Resistance | Tc | °C | 360 |
Volume Resistivity | 20°C | Ω.cm20°C | > 1012 |
Blade of textile