Welcome to ECBAY
refractory fire clay bricks(SK32,34,36,38)
refractory fire clay bricks(SK32,34,36,38)

1.type: SK32,34,36,38 2.refractoriness: >1710C 3.bulk density: >2.05g.cm3 4.porosity: >20% 5.size: STD or shaped

Item

SK-32

SK-34

SK-36

SK-38

Al2O3 (%)

35

38

55

70

Fe2O3 (%)

3.00

2.50

2.00

2.00

Refractoriness(SK)

32

34

36

38

Refractoriness

1710

1730

1760

--

Refractoriness under load0.2MPa

1300

1350

1450

1520

Porosity (%)

22-26

20-24

20-23

20-22

Bulk density (g/cm3)

2.05

2.10-2.2

2.25-2.35

2.40-2.50

Cold crushing strength (MPa)

22

25

45

50

Thermal expansion at 1000°C (%)

0.6

0.6

0.3

0.2

Clay bricks use Chamotte that the fire clay is calcinated as the main material. These bricks consist of fire clay and binder.

 The main applications are the low temperature parts such as blast furnaces and hot blast furnaces, waste incinerators and glass melting furnaces

refractory fire clay bricks(SK32,34,36,38)

Ads by Google


About Us | Contact Us | Help | Terms & Conditions