Welcome to ECBAY
Glassfiber Reinforced PP Plastic Particles
Glassfiber Reinforced PP Plastic Particles

Glassfiber Reinforced PP 1.monthly 800 tons 2.MOQ:1 TON or MORE 3.any color and percentage of GF as you require 4.UL SGS CSA

Glassfiber Reinforced PP1.introduction

 

(ITEM) 

(UNIT) 

(STANDARD) 

G15

G20

G30

G40

G30-B

G30-I

 

Tensile Strength

MPa

ISO 527-2

60

70

80

85

70

55

 

Tensile Elongation

%

ISO 527-2

-

-

-

-

-

-

 

Flexural Strength

MPa

ISO 178

85

90

105

110

95

70

Flexural Module

MPa

ISO 178

3500

4800

5500

6000

5000

4000

Charpy Notch Impact

KJ/m2

ISO 179-1

9.5

11

15

15

22

40

Izod Notch Impact

KJ/m2

ISO 180

7

9.5

13.5

13

20

36

Mass Density

g/cm3

ISO 1183

0.99

1.03

1.12

1.23

1.12

1.1

H.D.T

°C

ISO 75

130

145

150

150

145

135

Shrinkage For Injection Molding

%

GB/T-15585

0.7-1.0

0.5-0.8

0.5-0.8

0.5-0.8

0.5-0.8

0.5-0.8

Characteristics

 

 

general

general

general

high rigidity

high impact

high impact

 

 

 

 

 

 

 

 

 

 

2.Enhanced PP    Main use: widely used in the automotive industry, car manufacturing before the guard, after the car hood, heater housing, etc.; for the electrical industry, manufacturing, instrument case, battery boxes, etc.; for the chemical industry, manufacture of metering pumps, corrosion-resistant pipe Road, and frame filter shell. Provides low temperature grade and high flow grade. 3.Recommended processing conditions:

Drying temperature :90-100 ,2-4H Feeding section: 200 ~ 210 °C the middle section: 210 ~ 240 °C nozzle section: 210 ~ 230 °C Injection pressure of 50 ~ 80MPa Holding pressure 40 ~ 60 Mpa Mold temperature 30 ~ 60 °C

Glassfiber Reinforced PP Plastic Particles

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.