PRINTING CHEMICALS
PRINTING CHEMICALS

DEVELOPING OFFSET PRINTING PLATE

Features:1) 5 liters develops 250m2 of PS plate2) Short clean out time3) Sharp dots and clear background4) Little harm to oxidation layer and light-sensitive layer5) Durable6) Does not crystallize

DEVELOPMENT:  

BRAND: AOGUANG

MIX RATIO:

STEP 1:

DEVELOPER POWDER : WATER = 1 : 10

STORE THE CONCENTRATING LIQUID IN A SEALED PAIL, DON’T EXPOSE THE LIQUID IN THE AIR.

STEP 2:

1)       CONCENTRATING LIQUID : WATER = 1 : 5  WHEN DEVELOPER THE PLATE MANUALLY.

2)       CONCENTRATING LIQUID : WATER = 1 : 4  WHEN DEVELOPER THE PLATE BY MACHINE

TO AVOID DELIQUESCENCE, DON’T OPEN THE PACKAGE WHEN IT IS NOT USED.

DEVELOPING TEMPERATURE: 23±2°C 

NOTICE: HIGH TEMPERATURE WILL CAUSE THE WEB RESTORING AND PRESSRUN TO BECOME WORSE,BUT TOO LOW TEMPERATURE IS NOT ENOUGH FOR DEVELOPING OUT.

DEVELOPING TIME: 25-30 SECONDS (MACHINE)  30-50 SECONDS (MANUAL)

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.