thermal insulation brick
DKJL CO., LTD. [China]
1. Low thermal conductivity 2. Low thermal capacitance 3. Low impurity content 4. High hot compressive strength
Items | Testing Temperature(°C)When reheated with 2% contracting rate | Volume Densityg/cm3 | Pressure StrengthMpa | Thermal Conductivitykcal/mh°C(350°C) | |
A | A-1 | 900 | ≤0.50 | ≥0.50 | ≤0.13 |
A-2 | 1000 | ≤0.50 | ≥0.50 | ≤0.14 | |
A-3 | 1100 | ≤0.50 | ≥0.50 | ≤0.15 | |
A-4 | 1200 | ≤0.55 | ≥0.80 | ≤0.16 | |
A-5 | 1300 | ≤0.60 | ≥0.80 | ≤0.17 | |
A-6 | 1400 | ≤0.70 | ≥1.00 | ≤0.20 | |
A-7 | 1500 | ≤0.75 | ≥1.00 | ≤0.22 | |
B | B-1 | 900 | ≤0.70 | ≥2.50 | ≤0.17 |
B-2 | 1000 | ≤0.70 | ≥2.50 | ≤0.18 | |
B-3 | 1100 | ≤0.75 | ≥2.50 | ≤0.20 | |
B-4 | 1200 | ≤0.80 | ≥2.50 | ≤0.22 | |
B-5 | 1300 | ≤0.80 | ≥2.50 | ≤0.23 | |
B-6 | 1400 | ≤0.90 | ≥3.00 | ≤0.27 | |
B-7 | 1500 | ≤1.00 | ≥3.00 | ≤0.31 | |
C | C-1 | 1300 | ≤1.10 | ≥5.00 | ≤0.30 |
C-2 | 1400 | ≤1.20 | ≥7.00 | ≤0.38 | |
C-3 | 1500 | ≤1.25 | ≥10.00 | ≤0.45 |
thermal insulation brick