Highly water reducing concrete additives with retarding effect Suitable for working condition under temperature 5-40 centigrade

 Description

JK-08NP is a water reducing, highly effective superplasticizer additives with a set retarding effect for concrete in hot temperature which delays concrete setting time. It has also high range water reducing for promoting high early and ultimate strengths of concrete.

JK-08NP is naphthalene-based superplasticizer compounded by some of high-performance retarder, stabilizer and reinforcing admixtures etc.

It complies with ASTM C 494 Type G, GB8076-2008 and GB50119-2003.

Specifications

Item

Norm

Item

Norm

Appearance

Lark powder

Fluidity of cement

230mm

Fineness (0.315mm remains) %

≤12%

Chlorine content

Non

PH value

7-9

Moisture %

8.0 max

Uses

JK-08NP is ideal concrete admixtures for preparing high-performance and high-strength concrete, mass concrete and long-distance transport concrete etc.It is suitable for working condition under temperature 5-40 centigrade degree.Not suitable for being solely applied in the steam curing concrete.Test before applied in anhydrite, dross or similar industrial waste cement.AdvantageHas a high efficiency water-reducing, retarding in the initial setting and early strength in final setting, late-enhanced, less slump loss etc. which is extremely beneficial to the transport and to pouring of concrete.Increases initial workability. High ultimate strengths.The concrete of compressive strength, flexural, tensile, impermeability and durability are significantly improved and enhanced.The concrete setting time prolong 1-3h, it can also be adjusted according to the user's demand. It has not affected the strength growth of concrete at different time. Dosage 0.5-1.2% by weight of cement. Exact dosage rates are dependent on the type of effect sought, quality of cement and aggregates, water/cement ratio and ambient temperature. Therefore, in many cases it is advisable to carry out trial mixes.Using during mixing and after-mixing method and properly prolong stirring time to assure even.

Water reducing and Set retarding concrete additives

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.