1):Spec:1-100mm 2):coating way: ED-coat(gray,black) 3):spray(black),dipping coat 4):precise dimensional control
Provide ndfeb magnets is pressing bond by fast quenching NdFeB magnetic powder and adhesive through the "pressure molding" made of magnets.The size of the high precision bonded magnets,can make it forms.
A:Spec:1-100mm
B:Magnetization: radiation magnetizing,
axial magnetizing,
complanate magnetizing,
oblique magnetizing,
C:coating way: ED-coat(gray,black)
spray(black)
dipping coat
Magnetic and Physical Properties of Bonded Compression Moulding NdFeB | |||||||||||
DSM-4 | DSM-6 | DSM-8L | DSM-8 | DSM-8H | DSM-8SR | DSM-9L | DSM-9 | DSM-10 | DSM-11L | DSM-11 | |
Br (mT) | 400-500 | 500-600 | 600-650 | 600-680 | 600-650 | 600-650 | 600-680 | 680-730 | 700-750 | 760-810 | 780-830 |
Residual Induction (KGs) | (4.0-5.0) | (5.0-6.0) | (6.0-6.5) | (6.0-6.8) | (6.0-6.5) | (6.0-6.5) | (6.0-6.8) | (6.8-7.3) | (7.0-7.5) | (7.6-8.1) | (7.8-8.3) |
Hcb (KA/m) | 240-320 | 320-400 | 360-440 | 360-440 | 400-480 | 400-480 | 400-480 | 400-480 | 400-480 | 400-480 | 400-480 |
Coercive Force (Koe) | (3.0-4.0) | (4.0-5.0) | (4.5-5.5) | (4.5-5.5) | (5.0-6.0) | (5.0-6.0) | (5.0-6.0) | (5.0-6.0) | (5.0-6.0) | (5.0-6.0) | (5.0-6.0) |
Hcj (KA/m) | 560-720 | 560-720 | 640-800 | 640-800 | 1040-1360 | 960-1120 | 640-800 | 640-800 | 640-800 | 480-640 | 480-640 |
Intrinsic Coercive Force | (7.0-9.0) | (7.0-9.0) | (8.0-10.0) | (8.0-10.0) | (13.0-17.0) | (11.0-14.0) | (8.0-10.0) | (8.0-10.0) | (8.0-10.0) | (6.0-8.0) | (6.0-8.0) |
(BH)max (KJ/m3) | 32-44 | 52-60 | 60-68 | 64-72 | 60-68 | 60-68 | 68-76 | 76-84 | 80-88 | 84-92 | 88-96 |
Max. Energy Product | (4.0-5.5) | (6.5-7.5) | (7.5-8.5) | (8.0-9.0) | (7.5-8.5) | (7.5-8.5) | (8.5-9.5) | (9.5-10.5) | (10.0-11.0) | (10.5-11.5) | (11.0-12.0) |
1.2 | 1.3 | 1.3 | 1.2 | 1.16 | 1.16 | 1.2 | 1.2 | 1.2 | 1.2 | 1.2 | |
Permeability (Μh/M) | |||||||||||
(%/°C) | -0.11 | -0.11 | -0.11 | -0.11 | -0.08 | -0.08 | -0.11 | -0.1 | -0.1 | -0.11 | -0.11 |
Tempetrature Coefficient | |||||||||||
(°C) | 360 | 360 | 360 | 360 | 320 | 320 | 360 | 360 | 360 | 320 | 320 |
Curie Temperature | |||||||||||
(°C) | 130 | 130 | 130 | 130 | 160 | 160 | 130 | 130 | 130 | 120 | 120 |
Max.Operating Temperature | |||||||||||
(KA/m) | >1600 | >1600 | >1600 | >1600 | >2400 | >2000 | >1600 | >1600 | >1600 | >1600 | >1600 |
Magnetizing Force | >20 | >20 | >20 | >20 | >30 | >25 | >20 | >20 | >20 | >20 | >20 |
(g/m3) | 5.2-5.7 | 5.5-6.0 | 5.8-6.1 | 5.8-6.1 | 5.8-6.1 | 5.8-6.1 | 5.8-6.1 | 5.8-6.1 | 6.0-6.3 | 6.0-6.3 | 6.1-6.4 |
Dendity | |||||||||||
40-45 | 40-45 | 35-38 | 35-38 | 35-38 | 35-38 | 35-38 | 35-38 | 35-38 | 35-38 | 35-38 | |
Hardness |
permanent magnetic lamination motor wind generator