JK-15 is naphthalene-based non-corrosive, non-chlorine compound antifreeze admixture which compounded with water-reducing, early-strength, reducing the freezing point, preventing freezing damage etc. ingredients, powder, it has early-strength, water-reducing, air-entraining, anticorrosion etc. functions. It is mixed to the concrete according to the request, can obviously improve the configuration of the capillary pores and reduce free-water and the freezing point of the concrete effectively. And it can accelerate cement hydration and concrete hardening under the low temperature condition, enhance the early strength greatly and make the strong more and more by time, is ideal admixture for construction in winter.

Uses

JK-15 is suitable for the winter construction (in ambient temperatures ranging from -5 °C degree  to -20 °Cdegree) of common concrete, pumping concrete, large volume concrete and ready mixed concrete.

Advantage

JK-15 is a new generation of high efficient anti-freezing admixture. Small dosage, completely water soluble, low alkali, apparent reducing effect on the alkali-aggregate reaction. It can improve the workability, pumping properties and early strength of the concrete.JK-15 is suitable for concrete and precast below C50 but also the concrete above C50 with a addition of our high range water reducing admixture.

 

Specifications

Item

Norm

Item

Norm

Appearance

Lark powder

Fluidity of cement

120-160mm

Moisture

≤10%

Chlorine content

Non

PH value

7-9

Alkali content %

2.2

 

 

 

Technical Data Sheet

Item

JK-15 C10

JK-15 C15

JK-15 C20

Dosage

  2.0%

3.0%

4.0%

Lowest Daily Temperature

-5 °Cdegree

-10 °Cdegree

-15 °Cdegree

Setting Time Difference (min)

Initial

-60~+120

Final

Compressive Strength (Mpa)

1 day

8

2

1

3 days

25

20

10

7 days

40

30

15

28 days

60

50

40

Shrinkage (%)

28 days

≤120

Steel-bar Corrosion

None

Cautious

After the pouring construction covers the surface using the plastic sheeting and the grass curtain, do not let it to freeze immediately or blow the winds excessively caused the crack. Entering the mold temperature control above 5 °C degree.

Required heating curing at the early strength fast-enhancement. After the concrete formed, if the surface iced up, this phenomenon does not cause any the freezing damage. The intensity will remain enhancing rapidly, when the ambient temperature increasing

Antifreezing Concrete Admixture

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.