42.5 HSR sulfate resistance cement
42.5 HSR sulfate resistance cement

Erosion resistance capability, low resistance, good hydration heat, suitable for the erosion by sulfate harbor, wharf, undergrou  

Test Items

unit

National standard

Test result

conclusion

tricalcium silicate

%

≤ 50.0

46.6

Qualified

tricalcium aluminate

%

≤ 3.0

2.3

Qualified

loss on  lgnition

%

≤3.0

2.5

Qualified

magnesium oxide

%

≤ 5.0

3.7

Qualified

sulfur trioxide

%

≤ 2.5

2.2

Qualified

Insoluble residue

%

≤ 1.5

1.05

Qualified

Specific surface

m2/kg

≥280

423

Qualified

soundness

/

qualified

Qualified

initial setting time

Min

≥45

170

Qualified

final setting time

Min

≤600

230

Qualified

Alkali content*

%

≤0.6

/

Qualified

Sulfate resistance

%

≤0.04

0.025

Qualified

bending strength

ISO

3 days

Mpa

≥3.0

5.1

Qualified

28 days

≥6.5

7.2

Qualified

Compressive strength

3 days

Mpa

≥15.0

24.0

Qualified

28 days

≥42.5

46.0

Qualified

42.5 HSR sulfate resistance cement

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.