 They are widely to apply in cement building materials, power industry. During the process of production, under the conditions of single warehouse as well as normal mining: 40 grams are needed by per ton of cement as national standard; 30 grams as our enterprise; according to the feedback of the patrons, that's only need 18-19grams.

     Chemical composition<%>

Name

C

Si

Mn

Cr

Mo

Cu

S

P

high chrome alloy cast grinding micro-bar

1.7-3.2

0.3-1.2

1.0-2.6

10-16

0-0.5

0-0.5

≤0.08

≤0.10

    

      Mechanical properties of products       

 Name

Microstructure

Hardness<HRC>

high chrome alloy cast grinding micro-bar

M+C

≥56

       

       Specification

Φ8<mm>

Φ10<mm>

Φ12<mm>

Φ14<mm>

Ads by Google


About Us | Contact Us | Help | Terms & Conditions
Hot Products: A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | 0-9
Copyright Notice @ 2008-2022 ECBAY Limited and/or its subsidiaries and licensors. All rights reserved.